Wood adhesive(Urea formaldehyde resin)

Wood adhesive(Urea formaldehyde resin)

重庆市, 中国
生产能力:
3000 吨 / 月
重庆市, 中国
公司
86-023-53371333
13509028337
Chunyu Fung
联系人姓名

基本信息

分类 其他的粘合剂
化学文摘社编号. 9011-05-6
其他的名字 formaldehyde-urea resin
小额信贷 (CH4NO2.CH2O) x
出生地 Chongqing China (Mainland)
使用 Construction
牌子的名字 BENXON
模式的数量 wood powder
Woodadhesive (Urea formaldehyde resin)isone kind of Urea-formaldehyde resin powder Use Furniture assembly, wood veneer, wood sheet of laminated, curved wood adhesives, wood adhesive Feature 1. Wood adhesive is made by the urea-formaldehyde resin powder, the reinforcing agent and the curing agent. 2. Under the conditions of the cold bonding, thermal bonding, and high-frequency heating, after the curing agent mixed with the appropriate modifier (such as flour), can be used in the glue industry. 3. Wood powder isn’t being flammable. Specifications AppearanceWhite, free flowing powder Viscosity (glue: water = 2:1) (5000±500)mPa.s PH (glue: water = 2:1) 7.25±0.25 Proportion (glue: water = 2:1) about 1.290g/cm ³ Package Standard bag, net weight 20kg Storage 1. The woodadhesive is sealed in original containers.2. Suitable temperature3. Stored in dry placePreparation of rubber mixture 1. Water heated to a suitable temperature 2. The wood glue dissolved in warm water 3. Adding the curing agent after the mixture cool Glue mixture ratios (by weight) Wood powder 100Water 50±10Activity of When the temperature below 30 °C, the activity of glue is between 1 to 2 hours Wood preparation 1. Board thickness is uniform 2. Wood surfacekeeps clean 3. Wood moisture content was (9±3) %Adhesive volume It depends on the amount ofglue bonding material surface quality, the general amount is (175±25) g / m². Pressure Pressure depends on the surface of the material's density, surface smoothness, thickness tolerances, as well as paving the time. Normal pressure is 0.5-1.6MPa (5-16kg/cm ³)Pressure time Typically, when the temperature between 25 to 35 °C, the pressure test time is between 6 to 7 hours. Clean Rubber mixing equipment and coating equipment should be cleaned with warm waterSafety precautions 1. Please wear gloves, avoid direct contact with the glue. 2. Under good ventilation conditions, to prevent splashing into eyes. 3. Before and after operation, keeping clean.

交货条款及包装

Packaging Detail: 25KG/BAG Delivery Detail: 30 days after receipt of deposit
端口: Chongqing, Shanghai

付款条款

Documents Against Acceptance

Documents Against Payment

Letter of credit

Telegraphic transfer

Фотографии

    密码恢复
    要恢复您的密码,请在下面您的电子邮件地址框与您已注册请输入:
    The password reset code has been sent to your Email.
    Код уже был отправлен Вам ранее.
    Вы можете ввести его в поле выше, или получить новый код через сек.
    发生了错误。请检查您的电子邮件地址,然后再试一次。
    Ваш новый пароль:

    名称为空


    Выберите страну доставки

    您还没有写消息

    By clicking on the "Send" button, you agree that your data will be used to process your request. Further information and revocation instructions can be found in the data protection declaration.

    已发送您的消息!

    親密

    1
    Рынок B2B
    取消
      查看更多
        地區搜索
        全球
        Категории
          产品名称