Semi-Treated Fluff Pulp Pulping Process: Kraft Bleaching Process: ECF Wood Species: Southern Pine Typical Properties Average Fiber Length Length Weighted (mm): 2.7 Weight Weighted (mm): 3.4 Basis Weight (g/m2): 685 Caliper (mm): 1.29 Density (g/cc): 0.53 Mullen (kPa): 700 Moisture (%): 8 Extractives: 0.08 Brightness (ISO): 88.0 Kamas Energy (kWh/ton): 30 Fiberization (%): 100 Specific Absorption (sec/g): 0.95 Specific Capacity (g/g): 10.0 Packaging: Roll Diameter (cm): 116-152 Roll Width (cm): 25-152 Core Diameter (cm): 7.6