出生地 |
Guangdong China (Mainland) |
Process Parameter: Equipment for laminating film: dry and wet film laminator Temperature: Normal: 85 100 oC Special: 100 110 oC Roller pressure: 10 18 Mpa Speed: 8 50 m/min Remarks: Special laminations refer to those with thicker ink, solid color, high moisture content and bigger size paper. Application manual: 1. Adjust roller pressure and temperature according to different types of paper and ink. 2. When using the film for the first time or changing to other sixes, we recommend a small trial volume before going into fully mass lamination. 3. The following situation will affect the quality of the film during lamination. a. When using metal ink b. When the ink contains too much wax, dried oil, adhesive, and silicon additive.etc. c. When the ink is too thick. d. When the ink is not completely dry. e. When the paper contains too much moisture. f. When there is too much powder.Specificion & Parameter Specification 25uGLOSS Thickness(μm) Total 25 Base 12 Adhesive 13 Weight m(2)/kg 43.22 Kg/m(2) 0.0231 Width(mm) 36039044054059078088010801320140016001800(orascustomers'requset) Length(m) 200 3000 Papercore 25.4mm(1inch)58mm(2.25inch)76mm(3inch) Bonding Lessthan2 TensileStrength MD:2.4*10(6) dyne/cmCD:5.3*10(6)dyne/cm